Pt-Al涂层对一种镍基单晶高温合金抗热腐蚀行为的影响 |
|||||||||||||||
| 王迪, 王栋, 谢光, 王莉, 董加胜, 陈立佳 | |||||||||||||||
|
Influence of Pt-Al Coating on Hot Corrosion Resistance Behaviors of a Ni-Based Single-Crystal Superalloy |
|||||||||||||||
| WANG Di, WANG Dong, XIE Guang, WANG Li, DONG Jiasheng, CHEN Lijia | |||||||||||||||
| 表2 Pt-Al涂层试样热腐蚀前后截面组织数据统计 (μm) |
|||||||||||||||
| Table 2 Statistics of thicknesses of cross-sectional structure of Pt-Al coating sample intial and after hot corrosion test |
|||||||||||||||
|
|||||||||||||||