Pt-Al涂层对一种镍基单晶高温合金抗热腐蚀行为的影响 |
| 王迪, 王栋, 谢光, 王莉, 董加胜, 陈立佳 |
|
Influence of Pt-Al Coating on Hot Corrosion Resistance Behaviors of a Ni-Based Single-Crystal Superalloy |
| WANG Di, WANG Dong, XIE Guang, WANG Li, DONG Jiasheng, CHEN Lijia |
| 图7 在常压炉中900℃热腐蚀140 h后无涂层和Pt-Al涂层试样截面的SEM像及EPMA元素分布 |
| Fig.7 SEM images and EPMA element distributions of uncoated (a) and Pt-Al coating (b) samples cross-section in atmosphere furnace at 900oC for 140 h hot corrosion test |
|