Pt-Al涂层对一种镍基单晶高温合金抗热腐蚀行为的影响 |
| 王迪, 王栋, 谢光, 王莉, 董加胜, 陈立佳 |
|
Influence of Pt-Al Coating on Hot Corrosion Resistance Behaviors of a Ni-Based Single-Crystal Superalloy |
| WANG Di, WANG Dong, XIE Guang, WANG Li, DONG Jiasheng, CHEN Lijia |
| 图3 在常压炉中900℃热腐蚀过程中无涂层和Pt-Al涂层试样质量变化曲线 |
| Fig.3 Mass change curves of uncoated and Pt-Al coating samples in atmosphere furnace at 900oC hot corrosion test |
|