预变形与等温时效耦合作用下Ti-10Mo-1Fe/3Fe层状合金的力学性能 |
| 戴进财, 闵小华, 周克松, 姚凯, 王伟强 |
|
Coupling Effect of Pre-Strain Combined with Isothermal Ageing on Mechanical Properties in a Multilayered Ti-10Mo-1Fe/3Fe Alloy |
| DAI Jincai, MIN Xiaohua, ZHOU Kesong, YAO Kai, WANG Weiqiang |
| 图12 Ti-10Mo-1Fe、Ti-10Mo-3Fe合金和Ti-10Mo-1Fe/3Fe层状合金不同试样的拉伸性能及β钛合金塑性变形方式与力学性能的关系 |
| Fig.12 Tensile properties of Ti-10Mo-1Fe, Ti-10Mo-3Fe alloys, and Ti-10Mo-1Fe/3Fe multilayered alloy in the present study (a), and relationship between deformation modes and mechanical properties of β titanium alloys (b) |
|