预变形与等温时效耦合作用下Ti-10Mo-1Fe/3Fe层状合金的力学性能 |
| 戴进财, 闵小华, 周克松, 姚凯, 王伟强 |
|
Coupling Effect of Pre-Strain Combined with Isothermal Ageing on Mechanical Properties in a Multilayered Ti-10Mo-1Fe/3Fe Alloy |
| DAI Jincai, MIN Xiaohua, ZHOU Kesong, YAO Kai, WANG Weiqiang |
| 图9 Ti-10Mo-1Fe/3Fe层状合金ST试样的二次电子像和合金元素EDS线分析图 |
| Fig.9 Secondary electron image (a) and elemental distribution images of Ti (b), Mo (c), and Fe (d) measured by EDS along the black line in ST sample for Ti-10Mo-1Fe/3Fe multilayered alloy (The analyzed plane is normal to the TD) |
|