预变形与等温时效耦合作用下Ti-10Mo-1Fe/3Fe层状合金的力学性能 |
| 戴进财, 闵小华, 周克松, 姚凯, 王伟强 |
|
Coupling Effect of Pre-Strain Combined with Isothermal Ageing on Mechanical Properties in a Multilayered Ti-10Mo-1Fe/3Fe Alloy |
| DAI Jincai, MIN Xiaohua, ZHOU Kesong, YAO Kai, WANG Weiqiang |
| 图5 Ti-10Mo-1Fe和Ti-10Mo-3Fe合金ST试样不同拉伸变形量下的原位LSCM像 |
| Fig.5 In situ LSCM images of ST sample after 0 (a, e), 1% (b, f), 3% (c, g), and 5% (d, h) tensile strains for Ti-10Mo-1Fe (a-d) and Ti-10Mo-3Fe (e-h) alloys (The observed plane is normal to the transverse direction (TD), RD—rolling direction, ND—normal direction) |
|