预变形与等温时效耦合作用下Ti-10Mo-1Fe/3Fe层状合金的力学性能 |
| 戴进财, 闵小华, 周克松, 姚凯, 王伟强 |
|
Coupling Effect of Pre-Strain Combined with Isothermal Ageing on Mechanical Properties in a Multilayered Ti-10Mo-1Fe/3Fe Alloy |
| DAI Jincai, MIN Xiaohua, ZHOU Kesong, YAO Kai, WANG Weiqiang |
| 图3 Ti-10Mo-1Fe、Ti-10Mo-3Fe和Ti-15Mo合金ST及STA (473~673 K)试样的Vickers硬度,及Ti-10Mo-1Fe合金ST、STA (623 K)试样的压痕SEM像 |