激光沉积法制备Ti/TNTZO层状材料及其组织性能 |
||||||||||||||||
| 张婷, 李仲杰, 许浩, 董安平, 杜大帆, 邢辉, 汪东红, 孙宝德 | ||||||||||||||||
|
Microstruture and Properties of Ti/TNTZO Multi-Layered Material by Direct Laser Deposition |
||||||||||||||||
| ZHANG Ting, LI Zhongjie, XU Hao, DONG Anping, DU Dafan, XING Hui, WANG Donghong, SUN Baode | ||||||||||||||||
| 表2 采用DLD工艺制备的CP-Ti、TNTZO与Ti/TNTZO合金拉伸性能 |
||||||||||||||||
| Table 2 Tensile properties of CP-Ti, TNTZO, and Ti/TNTZO fabricated by DLD |
||||||||||||||||
|
||||||||||||||||