激光沉积法制备Ti/TNTZO层状材料及其组织性能 |
| 张婷, 李仲杰, 许浩, 董安平, 杜大帆, 邢辉, 汪东红, 孙宝德 |
|
Microstruture and Properties of Ti/TNTZO Multi-Layered Material by Direct Laser Deposition |
| ZHANG Ting, LI Zhongjie, XU Hao, DONG Anping, DU Dafan, XING Hui, WANG Donghong, SUN Baode |
| 图4 采用DLD技术制备的CP-Ti、TNTZO合金微观组织及EBSD分析 (a, d) OM images, yz plane (b, e) SEM images, xz plane (c, f) inverse pole figures X (IPF-X) and phase images (insets) of EBSD analysis, xz plane |
| Fig.4 The microstructures and EBSD analyses of the DLDed CP-Ti (a-c) and TNTZO (d-f) alloy |
|