激光沉积法制备Ti/TNTZO层状材料及其组织性能 |
| 张婷, 李仲杰, 许浩, 董安平, 杜大帆, 邢辉, 汪东红, 孙宝德 |
|
Microstruture and Properties of Ti/TNTZO Multi-Layered Material by Direct Laser Deposition |
| ZHANG Ting, LI Zhongjie, XU Hao, DONG Anping, DU Dafan, XING Hui, WANG Donghong, SUN Baode |
| 图1 直接激光沉积(DLD)制备Ti/TNTZO层状材料流程图 |
| Fig.1 Flowchart for the preparation of Ti/TNTZO by direct laser deposition (DLD) |
|