变形对超高强贝氏体钢组织和力学性能的影响 |
| 刘曼, 胡海江, 田俊羽, 徐光 |
|
Effect of Ausforming on the Microstructures and Mechanical Properties of an Ultra-High Strength Bainitic Steel |
| LIU Man, HU Haijiang, TIAN Junyu, XU Guang |
| 图1 热模拟实验工艺示意图 |
| Fig.1 Schematic of thermal simulation experiment (Ms—martensite transformation start temperature) |
|