搅拌头转速对2507双相不锈钢搅拌摩擦加工组织及性能的影响 |
| 陈果, 王新波, 张仁晓, 马成悦, 杨海峰, 周利, 赵运强 |
|
Effect of Tool Rotation Speed on Microstructure and Properties of Friction Stir Processed 2507 Duplex Stainless Steel |
| CHEN Guo, WANG Xinbo, ZHANG Renxiao, MA Chengyue, YANG Haifeng, ZHOU Li, ZHAO Yunqiang |
| 图12 母材和不同搅拌头转速下2507双相不锈钢搅拌区表面极化曲线 |
| Fig.12 Surface polarization curves of base material and stir zone of friction stir processed 2507 duplex stainless steel at different tool rotation speeds (E—potential, i—current density) |
|