搅拌头转速对2507双相不锈钢搅拌摩擦加工组织及性能的影响 |
| 陈果, 王新波, 张仁晓, 马成悦, 杨海峰, 周利, 赵运强 |
|
Effect of Tool Rotation Speed on Microstructure and Properties of Friction Stir Processed 2507 Duplex Stainless Steel |
| CHEN Guo, WANG Xinbo, ZHANG Renxiao, MA Chengyue, YANG Haifeng, ZHOU Li, ZHAO Yunqiang |
| 图3 不同搅拌头转速下2507双相不锈钢搅拌摩擦加工区截面形貌的OM像 |
| Fig.3 Cross-sectional OM images of the processing zone of friction stir processed 2507 duplex stainless steel at different tool rotation speeds of 200 r/min (a), 300 r/min (b), 400 r/min (c), 500 r/min (d), and 600 r/min (e) and the locally enlarged morphologies of hole defects in the square areas in Fig.3a (f), Fig.3d (g), and Fig.3e (h) |
|