时效对Ti-50.8Ni-0.1Zr形状记忆合金显微组织、拉伸性能和记忆行为的影响 |
| 叶俊杰, 贺志荣, 张坤刚, 杜雨青 |
|
Effect of Ageing on Microsturcture, Tensile Properties, and Shape Memory Behaviors of Ti-50.8Ni-0.1Zr Shape Memory Alloy |
| YE Junjie, HE Zhirong, ZHANG Kungang, DU Yuqing |
| 图3 时效温度和时效时间对Ti-50.8Ni-0.1Zr合金抗拉强度和断后伸长率的影响 |
| Fig.3 Effects of ageing temperature and ageing time (tag) on tensile strength (Rm) (a) and elongation (A) (b) of Ti-50.8Ni-0.1Zr alloys |
|