时效对Ti-50.8Ni-0.1Zr形状记忆合金显微组织、拉伸性能和记忆行为的影响 |
| 叶俊杰, 贺志荣, 张坤刚, 杜雨青 |
|
Effect of Ageing on Microsturcture, Tensile Properties, and Shape Memory Behaviors of Ti-50.8Ni-0.1Zr Shape Memory Alloy |
| YE Junjie, HE Zhirong, ZHANG Kungang, DU Yuqing |
| 图2 不同温度和时间时效处理后Ti-50.8Ni-0.1Zr合金的拉伸曲线 |
| Fig.2 Tensile curves of Ti-50.8Ni-0.1Zr alloys aged at 300oC (a), 400oC (b), and 500oC (c) for 1-50 h, respectively (800oC, 0.5 h solid-solution treated sample is also shown in Fig.2c) |
|