RAP法制备AlSi7Mg合金半固态坯料研究 |
| 姜巨福, 张逸浩, 刘英泽, 王迎, 肖冠菲, 张颖 |
|
Research on AlSi7Mg Alloy Semi-Solid Billet Fabricated by RAP |
| JIANG Jufu, ZHANG Yihao, LIU Yingze, WANG Ying, XIAO Guanfei, ZHANG Ying |
| 图3 不同变形温度和变形量对AlSi7Mg铝合金半固态坯料的影响 (a) average grain size (D) (b) shape factor (f) |
| Fig.3 The influence of different deformation temp-eratures and deformation amounts on AlSi7Mg aluminum alloy semi-solid billet |
|