热导型等离子弧焊电弧物理特性和熔池动态行为
|
|
李子晗, 忻建文, 肖笑, 王欢, 华学明, 吴东升
|
The Arc Physical Characteristics and Molten Pool Dynamic Behaviors in Conduction Plasma Arc Welding
|
|
LI Zihan, XIN Jianwen, XIAO Xiao, WANG Huan, HUA Xueming, WU Dongsheng
|
|
表1 SUS304不锈钢主要物性参数
|
Table 1 Physical properties of SUS304 stainless steel used in this model
|
|
| Parameter | Unit | Value | Parameter | Unit | Value |
|---|
| Density | kg·m-3 | 6900 | Liquidus temperature | K | 1727 | | Viscosity | kg·m-1·s-1 | 5.9 × 10-3 | Solidus temperature | K | 1697 | | Specific heat (liquid state) | J·kg-1·K-1 | 720 | Boiling temperature | K | 3133 | | Specific heat (solid state) | J·kg-1·K-1 | 760 | Heat transfer coefficient | W·m-2·K-4 | 20 | | Latent heat of fusion | J·kg-1 | 2.47 × 105 | Coefficient of thermal expansion | K-1 | 1.5 × 10-4 | | Thermal conductivity (liquid state) | W·m-1·K-1 | 28.4 | Surface tension | N·m-1 | 1.8 | | Thermal conductivity (solid state) | W·m-1·K-1 | 33.2 | Surface tension gradient | N·m-1·K-1 | -4.3 × 10-4 |
|
|
|