热导型等离子弧焊电弧物理特性和熔池动态行为 |
| 李子晗, 忻建文, 肖笑, 王欢, 华学明, 吴东升 |
|
The Arc Physical Characteristics and Molten Pool Dynamic Behaviors in Conduction Plasma Arc Welding |
| LI Zihan, XIN Jianwen, XIAO Xiao, WANG Huan, HUA Xueming, WU Dongsheng |
| 图9 熔池上表面红外热成像图及熔池表面温度实验结果与模拟结果对比 |
| Fig.9 Thermography image of molten pool surface in local coordinate system x1O1y1 (a) and comparison of experimental and simulated temperatures of molten pool surface (b) |
|