热导型等离子弧焊电弧物理特性和熔池动态行为 |
| 李子晗, 忻建文, 肖笑, 王欢, 华学明, 吴东升 |
|
The Arc Physical Characteristics and Molten Pool Dynamic Behaviors in Conduction Plasma Arc Welding |
| LI Zihan, XIN Jianwen, XIAO Xiao, WANG Huan, HUA Xueming, WU Dongsheng |
| 图6 y0 = 0对称面熔池不同时间下的温度分布、流场分布及三维流速分布 |
| Fig.6 Distributions of temperature field, fluid flow field (a1-d1), and three-dimensional velocity field (a2-d2) at y0 = 0 at time t = 0.06 s (a1, a2), t = 0.38 s (b1, b2), t = 1.26 s (c1, c2), and t = 1.80 s (d1, d2) |
|