热导型等离子弧焊电弧物理特性和熔池动态行为 |
| 李子晗, 忻建文, 肖笑, 王欢, 华学明, 吴东升 |
|
The Arc Physical Characteristics and Molten Pool Dynamic Behaviors in Conduction Plasma Arc Welding |
| LI Zihan, XIN Jianwen, XIAO Xiao, WANG Huan, HUA Xueming, WU Dongsheng |
| 图3 等离子弧焊实验装置示意图 |
| Fig.3 Schematic sketch of experimental set-up of plasma arc welding |
|