表面喷丸处理对NiCrAlYSi涂层恒温氧化行为的影响 |
| 刘冠熙, 黄光宏, 罗学昆, 申造宇, 何利民, 李建平, 牟仁德 |
|
The Influence of Surface Shot Peening on the Isothermal Oxidation Behavior of NiCrAlYSi Coating |
| LIU Guanxi, HUANG Guanghong, LUO Xuekun, SHEN Zaoyu, HE Limin, LI Jianping, MU Rende |
| 图4 NiCrAlYSi涂层1050℃恒温氧化200和600 h后截面形貌的SEM像 (a, b) P-0 (c, d) P-1 (e, f) P-2 |
| Fig.4 Cross-sectional SEM images of NiCrAlYSi coating after 200 h (a, c, e) and 600 h (b, d, f) isothermal oxidation at 1050oC |
|