Fe含量对Zr60Cu40-xFex相分离非晶合金组织结构、电阻性能和纳米压痕行为的影响 |
| 孙小钧, 何杰, 陈斌, 赵九洲, 江鸿翔, 张丽丽, 郝红日 |
|
Effect of Fe Content on the Microstructure, Electrical Resistivity, and Nanoindentation Behavior of Zr60Cu40-xFex Phase-Separated Metallic Glasses |
| SUN Xiaojun, HE Jie, CHEN Bin, ZHAO Jiuzhou, JIANG Hongxiang, ZHANG Lili, HAO Hongri |
| 图7 纳米压痕力-位移(P-h)曲线 |
| Fig.7 Nanoindentation force-displacement (P-h) curves of Zr60Cu20Fe20, Zr60Cu40, and Zr75Fe25 alloys |
|