Fe含量对Zr60Cu40-xFex相分离非晶合金组织结构、电阻性能和纳米压痕行为的影响 |
| 孙小钧, 何杰, 陈斌, 赵九洲, 江鸿翔, 张丽丽, 郝红日 |
|
Effect of Fe Content on the Microstructure, Electrical Resistivity, and Nanoindentation Behavior of Zr60Cu40-xFex Phase-Separated Metallic Glasses |
| SUN Xiaojun, HE Jie, CHEN Bin, ZHAO Jiuzhou, JIANG Hongxiang, ZHANG Lili, HAO Hongri |
| 图6 Zr60Cu20Fe20合金富Zr-Fe基体及富Zr-Cu粒子在673 K等温退火0.5 h后的HRTEM像 (a) glassy Fe-rich matrix (the rectangular areas indicate the formation of nanocrystals) (b) glassy Cu-rich sphere |
| Fig.6 HRTEM images of as-quenched Zr60Cu20Fe20 alloys annealed at 673 K for 0.5 h |
|