Fe含量对Zr60Cu40-xFex相分离非晶合金组织结构、电阻性能和纳米压痕行为的影响 |
| 孙小钧, 何杰, 陈斌, 赵九洲, 江鸿翔, 张丽丽, 郝红日 |
|
Effect of Fe Content on the Microstructure, Electrical Resistivity, and Nanoindentation Behavior of Zr60Cu40-xFex Phase-Separated Metallic Glasses |
| SUN Xiaojun, HE Jie, CHEN Bin, ZHAO Jiuzhou, JIANG Hongxiang, ZHANG Lili, HAO Hongri |
| 图2 Zr60Cu40-xFex合金薄带样品微观组织的TEM像和SAED花样 |
| Fig.2 TEM images and corresponding SAED patterns (insets) of the as-quenched Zr60Cu40-xFex alloys with x = 12 (a) and x = 20 (b) |
|