5356铝合金TIG电弧增材制造组织与力学性能 |
| 孙佳孝, 杨可, 王秋雨, 季珊林, 包晔峰, 潘杰 |
|
Microstructure and Mechanical Properties of 5356 Aluminum Alloy Fabricated by TIG Arc Additive Manufacturing |
| SUN Jiaxiao, YANG Ke, WANG Qiuyu, JI Shanlin, BAO Yefeng, PAN Jie |
| 图5 WAAM 5356铝合金薄壁件最顶层的显微组织 (a) macrostructure of the top region of the thin-walled part (b) microstructure of the bottom of the top layer (c) microstructure of the middle and upper of the top layer |
| Fig.5 Macrostructure and microstructures of top region of the WAAM 5356 aluminum alloy thin-walled part |
|