5356铝合金TIG电弧增材制造组织与力学性能 |
| 孙佳孝, 杨可, 王秋雨, 季珊林, 包晔峰, 潘杰 |
|
Microstructure and Mechanical Properties of 5356 Aluminum Alloy Fabricated by TIG Arc Additive Manufacturing |
| SUN Jiaxiao, YANG Ke, WANG Qiuyu, JI Shanlin, BAO Yefeng, PAN Jie |
| 图1 WAAM 5356铝合金薄壁件制备过程示意图、试样截取示意图及拉伸试样几何尺寸 |
| Fig.1 Schematic of WAAM 5356 aluminum alloy thin-walled parts preparation process and sample interception (a) and tensile specimen geometry (b) |
|