用于燃料电池双极板的不锈钢成分优化
|
|
黄一川, 王清, 张爽, 董闯, 吴爱民, 林国强
|
Optimization of Stainless Steel Composition for Fuel Cell Bipolar Plates
|
|
HUANG Yichuan, WANG Qing, ZHANG Shuang, DONG Chuang, WU Aimin, LIN Guoqiang
|
|
表8 酸钝化和电化学氮化后设计合金的界面接触电阻
|
Table 8 Interfacial contact resistance (ICR) of the designed and reference alloys after acid passivation and electrochemical nitridation
|
|
| Cluster | Passivation method | ICR / (Ω·cm2) (0.064 MPa) |
|---|
| | Before | After | | [Ni-Fe12]Cr3 | Acid passivation | 0.26 | 1.16 | | [Ni-Fe11.5Ni0.5]Cr3 | Acid passivation | 0.27 | 1.12 | | [Ni-Fe11Ni]Cr3 | Acid passivation | 0.41 | 1.10 | | [Ni-Fe10.5Ni1.5]Cr3 | Acid passivation | 0.46 | 1.04 | | Electrochemical nitriding | 0.46 | 1.07 | | [Ni-Fe10Ni2]Cr3 | Acid passivation | 0.51 | 0.99 | | Electrochemical nitriding | 0.51 | 1.03 | | [Ni-Fe9Ni3]Cr3 | Acid passivation | 0.49 | 0.98 | | [Ni-Fe8Ni4]Cr3 | Acid passivation | 0.50 | 0.98 |
|
|
|