用于燃料电池双极板的不锈钢成分优化 |
| 黄一川, 王清, 张爽, 董闯, 吴爱民, 林国强 |
|
Optimization of Stainless Steel Composition for Fuel Cell Bipolar Plates |
| HUANG Yichuan, WANG Qing, ZHANG Shuang, DONG Chuang, WU Aimin, LIN Guoqiang |
| 图13 电化学氮化处理后合金的自腐蚀电位与自腐蚀电流密度随Ni当量的变化情况 |
| Fig.13 Ecorr and icorr of alloys after electrochemical nitridation vs their Ni equivalents |
|