用于燃料电池双极板的不锈钢成分优化 |
| 黄一川, 王清, 张爽, 董闯, 吴爱民, 林国强 |
|
Optimization of Stainless Steel Composition for Fuel Cell Bipolar Plates |
| HUANG Yichuan, WANG Qing, ZHANG Shuang, DONG Chuang, WU Aimin, LIN Guoqiang |
| 图7 设计合金与316L不锈钢经酸钝化处理前后在0.5 mol/L H2SO4 + 2 × 10-6 HF水溶液中的动电位极化曲线 |
| Fig.7 Dynamic potential polarization curves of the designed and reference alloys before (a) and after (b) acid passivation treatment in 0.5 mol/L H2SO4 + 2 × 10-6 HF aqueous solution (i—corrosion current density, E—potential) |
|