用于燃料电池双极板的不锈钢成分优化 |
| 黄一川, 王清, 张爽, 董闯, 吴爱民, 林国强 |
|
Optimization of Stainless Steel Composition for Fuel Cell Bipolar Plates |
| HUANG Yichuan, WANG Qing, ZHANG Shuang, DONG Chuang, WU Aimin, LIN Guoqiang |
| 图6 钝化处理前后的设计合金及参照合金开路电位-时间曲线 |
| Fig.6 Open circuit potential (Eocp)-time (t) curves of the designed and reference alloys before and after passivation treatment |
|