用于燃料电池双极板的不锈钢成分优化 |
| 黄一川, 王清, 张爽, 董闯, 吴爱民, 林国强 |
|
Optimization of Stainless Steel Composition for Fuel Cell Bipolar Plates |
| HUANG Yichuan, WANG Qing, ZHANG Shuang, DONG Chuang, WU Aimin, LIN Guoqiang |
| 图5 设计合金及316L不锈钢的硬度随Ni当量的变化情况 |
| Fig.5 Hardness of the the designed alloy and reference alloy (316L stainless steel) vs their Ni equivalents |
|