用于燃料电池双极板的不锈钢成分优化 |
| 黄一川, 王清, 张爽, 董闯, 吴爱民, 林国强 |
|
Optimization of Stainless Steel Composition for Fuel Cell Bipolar Plates |
| HUANG Yichuan, WANG Qing, ZHANG Shuang, DONG Chuang, WU Aimin, LIN Guoqiang |
| 图4 [Ni-Fe13-xNix-1]Cr3合金经固溶加水淬处理后显微组织的OM像 (a) [Ni-Fe12]Cr3 (b) [Ni-Fe11.5Ni0.5]Cr3 (c) [Ni-Fe11Ni]Cr3 (d) [Ni-Fe10.5Ni1.5]Cr3 (e) [Ni-Fe10Ni2]Cr3 (f) [Ni-Fe9Ni3]Cr3 (g) [Ni-Fe8Ni4]Cr3 |
| Fig.4 OM images of the designed alloys after solution and water-quenching treatment |
|