Laves相对 GH3625合金管材热挤压过程中爆裂行为的影响 |
| 陈建军, 丁雨田, 王琨, 闫康, 马元俊, 王兴茂, 周胜名 |
|
Effects of Laves Phase on Burst Behavior of GH3625 Superalloy Pipe During Hot Extrusion |
| CHEN Jianjun, DING Yutian, WANG Kun, YAN Kang, MA Yuanjun, WANG Xingmao, ZHOU Shengming |
| 图7 图6c中方框区域裂纹终端的SEM像和EDS面扫描 |
| Fig.7 SEM image and EDS map scan of crack terminal in square area of Fig.6c |
|