Laves相对 GH3625合金管材热挤压过程中爆裂行为的影响 |
| 陈建军, 丁雨田, 王琨, 闫康, 马元俊, 王兴茂, 周胜名 |
|
Effects of Laves Phase on Burst Behavior of GH3625 Superalloy Pipe During Hot Extrusion |
| CHEN Jianjun, DING Yutian, WANG Kun, YAN Kang, MA Yuanjun, WANG Xingmao, ZHOU Shengming |
| 图1 GH3625合金管材热挤压实验过程示意图 |
| Fig.1 Flow chart of hot extrusion experiment for the GH3625 superalloy pipe |
|