| 图6 FC态Fe50Mn30Co10Cr10高熵合金经拉伸变形后断口附近区域的TEM像及SAED花样 |
| Fig.6 TEM image (a) and corresponding SAED pattern (b) of the region close to the fracture surface of the deformed Fe50Mn30Co10Cr10 HEA at FC state showing ε-martensite laths and deformation twins |
|