非均匀组织FeMnCoCr高熵合金的微观结构和力学性能 |
| 王洪伟, 何竹风, 贾楠 |
|
Microstructure and Mechanical Properties of a FeMnCoCr High-Entropy Alloy with Heterogeneous Structure |
| WANG Hongwei, HE Zhufeng, JIA Nan |
| 图3 PC态Fe50Mn30Co10Cr10高熵合金在拉伸变形前后的EBSD像 (a1, a2) recrystallization region (b1, b2) deformed matrix-preserved region (c1, c2) the region close to the fracture surface of the alloy |
| Fig.3 Phase distribution maps (a1-c1) and orientation maps (a2-c2) of the Fe50Mn30Co10Cr10 HEA at the PC state before (a1, a2, b1, b2) and after (c1, c2) deformation taken from different regions (In the phase distribution maps, high-angle boundaries with misorientation angles larger than 10° are indicated by thick black lines, low-angle boundaries with misorientation angles between 3° and 10° are indicated by thin black lines, and Σ3 twin boundaries in the fcc phase are indicated by white solid lines, respectively; RD—rolling direction, ND—normal direction, LD—loading direction) |
|