非均匀组织FeMnCoCr高熵合金的微观结构和力学性能 |
| 王洪伟, 何竹风, 贾楠 |
|
Microstructure and Mechanical Properties of a FeMnCoCr High-Entropy Alloy with Heterogeneous Structure |
| WANG Hongwei, HE Zhufeng, JIA Nan |
| 图1 Fe50Mn30Co10Cr10高熵合金的室温拉伸力学性能 (a) engineering stress-strain curves of the HEA annealed at 650oC for different time periods (b) engineering stress-strain curves of the HEA at different states (c) true stress-strain curves (d) work hardening curves corresponding to Fig.1c |
| Fig.1 Mechanical properties of Fe50Mn30Co10Cr10 high-entropy alloy (HEA) under tensile testing at room temperature (HOMO—homogenization, PC—partially recrystallized, FC—fully recrystallized) |
|