镁空气电池阳极用挤压态Mg-2Bi-0.5Ca-0.5In合金的放电性能和电化学行为 |
| 程伟丽, 谷雄杰, 成世明, 陈宇航, 余晖, 王利飞, 王红霞, 李航 |
|
Discharge Performance and Electrochemical Behaviors of the Extruded Mg-2Bi-0.5Ca-0.5In Alloy as Anode for Mg-Air Battery |
| CHENG Weili, GU Xiongjie, CHENG Shiming, CHEN Yuhang, YU Hui, WANG Lifei, WANG Hongxia, LI Hang |
| 图11 在10和120 mA/cm2电流密度下放电不同时间段挤压态BXI200合金去产物的表面形貌 |
| Fig.11 Surface morphologies of the extruded BXI200 alloy without discharge products after discharge at 10 mA/cm2 (a, b) and 120 mA/cm2 (c, d) for 10 min (a, c) and 60 min (b, d) (Insets show the high magnified images) |
|