镁空气电池阳极用挤压态Mg-2Bi-0.5Ca-0.5In合金的放电性能和电化学行为 |
| 程伟丽, 谷雄杰, 成世明, 陈宇航, 余晖, 王利飞, 王红霞, 李航 |
|
Discharge Performance and Electrochemical Behaviors of the Extruded Mg-2Bi-0.5Ca-0.5In Alloy as Anode for Mg-Air Battery |
| CHENG Weili, GU Xiongjie, CHENG Shiming, CHEN Yuhang, YU Hui, WANG Lifei, WANG Hongxia, LI Hang |
| 图7 挤压态BXI200合金的等效电路图 |
| Fig.7 Equivalent circuit diagram of the extruded BXI200 alloy (Rs—solution resistance, Rct—charge transfer resistance, CPE—constant phase element, L—inductor, RL—inductance resistance, RE—reference electrode, WE—working electrode) |
|