镁空气电池阳极用挤压态Mg-2Bi-0.5Ca-0.5In合金的放电性能和电化学行为 |
| 程伟丽, 谷雄杰, 成世明, 陈宇航, 余晖, 王利飞, 王红霞, 李航 |
|
Discharge Performance and Electrochemical Behaviors of the Extruded Mg-2Bi-0.5Ca-0.5In Alloy as Anode for Mg-Air Battery |
| CHENG Weili, GU Xiongjie, CHENG Shiming, CHEN Yuhang, YU Hui, WANG Lifei, WANG Hongxia, LI Hang |
| 图1 挤压态Mg-2Bi-0.5Ca-0.5In (BXI200)合金的晶体取向图和(0001)极图 |
| Fig.1 Crystallographic orientation map (a) and (0001) pole figure (b) of the extruded Mg-2Bi-0.5Ca-0.5In (BXI200) alloy (ED—extrusion direction, TD—transverse direction) |
|