热处理对激光选区熔化AlSi10Mg合金显微组织及力学性能的影响 |
王悦, 王继杰, 张昊, 赵泓博, 倪丁瑞, 肖伯律, 马宗义 |
Effects of Heat Treatments on Microstructure and Mechanical Properties of AlSi10Mg Alloy Produced by Selective Laser Melting |
WANG Yue, WANG Jijie, ZHANG Hao, ZHAO Hongbo, NI Dingrui, XIAO Bolv, MA Zongyi |
图4 优化参数后SLM制备样品显微组织的OM像及SEM像 |
Fig.4 OM images of horizontal (a) and vertical (b) sections of the optimized SLM sample and SEM images corresponding to the two directions (c, d) (HAZ—hot affected zone) |
![]() |