热处理对激光选区熔化AlSi10Mg合金显微组织及力学性能的影响 |
| 王悦, 王继杰, 张昊, 赵泓博, 倪丁瑞, 肖伯律, 马宗义 |
|
Effects of Heat Treatments on Microstructure and Mechanical Properties of AlSi10Mg Alloy Produced by Selective Laser Melting |
| WANG Yue, WANG Jijie, ZHANG Hao, ZHAO Hongbo, NI Dingrui, XIAO Bolv, MA Zongyi |
| 图1 用于激光选区熔化(SLM)的AlSi10Mg粉末形貌 (a) surface morphology (b) cross section of a particle under high magnification |
| Fig.1 SEM images of AlSi10Mg powders for selective laser melting (SLM) |
|