过热度对轴承钢凝固组织整体形貌特征及渗透率的影响 |
| 曹江海, 侯自兵, 郭中傲, 郭东伟, 唐萍 |
|
Effect of Superheat on Integral Morphology Characteristics of Solidification Structure and Permeability in Bearing Steel Billet |
| CAO Jianghai, HOU Zibing, GUO Zhongao, GUO Dongwei, TANG Ping |
| 图8 分形维数与比表面积的关系 |
| Fig.8 Relationship between fractal dimension and specific surface area |
|