低应变预变形对变温马氏体相变行为的影响规律及作用机制 |
| 王金亮, 王晨充, 黄明浩, 胡军, 徐伟 |
|
The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation |
| WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei |
| 图7 奥氏体、ε-马氏体和α'-马氏体取向的低指数极图 (a) pole figure of γ (b) pole figure of ε-martensite (c) pole figure of α'-martensite |
| Fig.7 Pole figure comparisons between experiment (Red points, corresponding to the data obtained from square areas in Fig.6) and calculation (other symbols) for γ→ε→α' transformation (N.D. and R.D. refer to normal direction and rolling direction of sample, respectively) |
|