非晶合金粉末作为润滑油添加剂的摩擦学性能 |
| 毕甲紫, 刘晓斌, 李然, 张涛 |
|
Tribological Properties of Polyalphaolefin (PAO6) Lubricant Modified with Particles Additives of Metallic Glass |
| BI Jiazi, LIU Xiaobin, LI Ran, ZHANG Tao |
| 图6 添加不同浓度Mn55Fe25P10B7C3非晶合金粉末下磨斑白光干涉形貌、磨损深度变化曲线与白光干涉粗糙度变化 |
| Fig.6 WLI surface topographies of worn surfaces (a-f), worn depth (g), and roughness (Ra, RPV) of worn surfaces (h) with different concentrations of Mn55Fe25P10B7C3 MG powders (Ra—arithmetic mean deviation of roughness, RPV—maximum peak-to-valley roughness) |
|