非晶合金粉末作为润滑油添加剂的摩擦学性能 |
| 毕甲紫, 刘晓斌, 李然, 张涛 |
|
Tribological Properties of Polyalphaolefin (PAO6) Lubricant Modified with Particles Additives of Metallic Glass |
| BI Jiazi, LIU Xiaobin, LI Ran, ZHANG Tao |
| 图3 PAO6基础油中添加不同浓度Mn55Fe25P10B7C3非晶合金粉末下四球测试摩擦系数随时间变化曲线 |
| Fig.3 Variations of coefficient of friction vs time for PAO6 with different concentrations of Mn55Fe25P10B7C3 MG powders |
|