非晶态Ni80P20合金的玻璃转变和过冷液体性质 |
| 杨群, 彭思旭, 卜庆周, 于海滨 |
|
Revealing Glass Transition and Supercooled Liquid in Ni80P20 Metallic Glass |
| YANG Qun, PENG Sixu, BU Qingzhou, YU Haibin |
| 图4 升温速率为700 K/s时,通过高温传感器测量的Ni80P20金属玻璃的比热曲线及熔化热流曲线 |
| Fig.4 The specific heat capacity curve measured by a high temperature sensor (Inset is an enlarged view of the specific heat curve at the glass transition) (a), and the melting heat flow curve (b) of Ni80P20 metallic glass at a heating rate of 700 K/s (cp—special heat capacity, ΔHm—melting enthalpy, Δcp—heat capacity step) |
|