非晶态Ni80P20合金的玻璃转变和过冷液体性质 |
| 杨群, 彭思旭, 卜庆周, 于海滨 |
|
Revealing Glass Transition and Supercooled Liquid in Ni80P20 Metallic Glass |
| YANG Qun, PENG Sixu, BU Qingzhou, YU Haibin |
| 图3 Ni80P20金属玻璃分别在DSC和FSC的升温速率范围内的晶化Kissinger图,及不同升温速率下的玻璃转变温度的变化与VFT方程拟合 |
| Fig.3 The crystallization Kissinger diagram of Ni80P20 metallic glasses in the heating rate range of DSC and FSC respectively (a), and the change of glass transition temperature at different heating rates and the fitting of VFT equation (b) (Tx—crystallization temperature, Tg20—extrapolated Tg at a heating rate of 20 K/min, m—fragility) |
|