非晶态Ni80P20合金的玻璃转变和过冷液体性质 |
| 杨群, 彭思旭, 卜庆周, 于海滨 |
|
Revealing Glass Transition and Supercooled Liquid in Ni80P20 Metallic Glass |
| YANG Qun, PENG Sixu, BU Qingzhou, YU Haibin |
| 图2 Ni80P20金属玻璃在不同升温速率下的FSC热流曲线及Ni80P20金属玻璃在不同升温速率下的相图 |
| Fig.2 FSC heat flow curves (a) and phase diagram (b) of Ni80P20 metallic glass at different heating rates (SCL—supercooled liquid) |
|