具有异常放热现象的Fe-Nb-B-Y非晶合金燃烧机理 |
| 胡祥, 葛嘉城, 刘思楠, 伏澍, 吴桢舵, 冯涛, 刘冬, 王循理, 兰司 |
|
Combustion Mechanism of Fe-Nb-B-Y Amorphous Alloys with an Anomalous Exothermic Phenomenon |
| HU Xiang, GE Jiacheng, LIU Sinan, FU Shu, WU Zhenduo, FENG Tao, LIU Dong, WANG Xunli, LAN Si |
| 图4 Y4.5样品不同温度下以0.33 K/s的升温速率加热时有自放热过程、无自放热过程和以1.67 K/s的升温速率快速加热过程的结构因子S(Q)和约化对分布函数G(r) (a, d) plots for the sample with a self-heating process with heating rate 0.33 K/s (b, e) plots for the sample without self-heating during a normal slow heating process with heating rate 0.33 K/s (c, f) plots for the sample with a fast-heating rate (1.67 K/s) |
| Fig.4 S(Q) (a-c) and G(r) (d-f) plots of Y4.5 MGs under different temperatures (The G(r) plots illustrate that the crystalline products for the samples after heating with different rates are different. S(Q) |
|